If you’ve ever worked with liquid silicone rubber (LSR) molding, you know the pain: that perfect part you designed for a tight tolerance ends up 2-5% smaller right after ejection, and suddenly you’re retooling or trashing batches that cost you time and cash. As an LSR molder supplier, I’ve dealt with this a hundred times—from tiny medical seals that need to fit into a catheter to consumer electronics gaskets that can’t gap around a phone’s camera. Shrinkage isn’t a fluke; it’s a predictable (but fixable) part of the process, and today I’m breaking down exactly how to dial it in, without guessing or wasting material.

First, let’s cut to the basics: LSR shrinkage happens in two main phases, and if you only fix one, you’re leaving half the problem on the table. The first is post-cure shrinkage—that slow, 0.1-0.5% tightening that happens hours or even days after the part comes out of the mold, as the silicone’s cross-linked polymer chains settle down. The second is in-mold shrinkage, the bigger chunk (1-4%) that occurs when the part cools and is ejected. Mess up either, and you’re looking at parts that fail inspection or require endless tooling tweaks.

TYM-W LSR Injection Molding MachineTYM-W Toggle LSR Injection Molding Machine

Let’s start with the most controllable factor: your machine setup. I’ve seen guys use old, tired injection presses and wonder why their shrinkage is all over the place. Not all LSR machines are created equal. For example, toggle-style machines (like our top pick, the TYM-W Toggle LSR Injection Molding Machine) keep mold clamping pressure super consistent—no fluctuations mid-cycle, which is key for even material flow and cure. Wobbly pressure means some parts cure faster than others, leading to uneven shrinkage. I also swear by horizontal presses for LSR (you can check out our line here: TYM-W LSR Injection Molding Machine) because they let you tune shot size and injection speed way more precisely than vertical models, especially for small, detailed parts.

Wait, if you’re molding dual-color LSR or LSR with hard plastic inserts, you’ll want a machine built specifically for that. Our TYM-W55T200 2K / Double-Color Machine has a synchronized injection unit that keeps both materials curing at the same rate—no mismatched shrinkage that warps the bond between LSR and the insert. That’s a game-changer for medical devices or wearables where two materials have to lock tight.

Next, material selection and prep. LSR comes in different hardnesses (30 Shore A to 80 Shore A) and cure speeds, and the wrong grade will make shrinkage impossible to control. For example, fast-cure LSR might seem great for cycle time, but it cures too quick in the mold core, so the outer skin doesn’t set evenly—leading to post-cure shrinkage that’s off. I always recommend testing a medium-cure, high-consistency grade first (ask your material rep for “low-shrink LSR formulations”) because their cross-link density is more uniform. Also, don’t skip degassing your LSR before injection! Trapped air makes voids, which create uneven cooling and shrinkage. Most modern LSR machines have built-in degassing, but if you’re running an older press, spend 10 minutes vacuuming your material mix before loading—worth it for consistent parts.

Then, mold design and temperature control. This is where most molders cut corners, and it shows. Your mold’s temperature has to be rock solid—LSR cures when it hits a specific temp, so even a 5°F difference between the cavity and core can make one side shrink more than the other. I use cartridge heaters in the mold, set to 350-380°F (depending on material), with a precision thermocouple that updates every second—no dial thermostats that drift. Also, leave a tiny “shrinkage allowance” in your mold. A lot of designers forget to add this, so they make the mold exactly the size they want the part, but LSR shrinks. Rule of thumb: for most general-purpose LSR, add 1.5-2% to all dimensions. For high-tolerance parts (like medical seals, which need ±0.005mm), bump that up to 2.2-2.5%, then adjust after testing 10-15 parts.

Ejection timing is another underrated trick. If you eject the part too early, it’s still soft, so it compresses as you push it out—then shrinks way more when it cools. If you eject too late, it sticks to the mold (bad news for cycle time) and might develop stress that causes uneven shrinkage. I use a trial-and-error method here: for a basic 10mm-thick part, wait 15-20 seconds after injection before ejecting. For thicker parts (over 20mm), add 5 seconds per extra mm to make sure the core is fully cured. Also, make sure your ejector pins are sized right—too big, and you’ll mark the part or compress it; too small, and ejection is uneven.

Post-cure is where you can fine-tune shrinkage after the part is out of the mold, but do it right. A lot of guys toss parts in an oven at 300°F for 30 minutes, but that’s a one-size-fits-all approach. For low-shrink parts, use a “step-cure” profile: start at 200°F for 1 hour to let the cross-links stabilize, then ramp up to 300°F for 2 hours. That way, you’re not shocking the silicone, which can cause uneven shrinkage. If you’re dealing with parts that shrink too much post-mold, try a 10-minute “relaxation hold” at room temp before post-cure—this lets the polymer chains settle slowly, so they don’t contract all at once.

Now, let’s talk about troubleshooting common issues. If your parts are shrinking more on one side, check mold temperature first—you probably have a cold spot in the cavity. If all parts are shrinking too much, your mold shrinkage allowance is too low, or you’re using a too-fast cure speed. If shrinkage is inconsistent batch to batch, your injection pressure is fluctuating, or you’re not degassing the material properly. I once had a customer who was getting 4% shrinkage on tiny O-rings—turns out he was using an old machine with a worn injection screw, so the shot size was off by 0.5cc every cycle. Swapping to one of our TYM-W LSR Injection Molding Machine models fixed it instantly, no more guesswork.

Here’s a pro tip I learned from 10 years in the game: keep a log for every job. Write down mold temperature, injection pressure, shot size, cure time, and actual shrinkage rate for 20-30 test parts. After 5 jobs, you’ll start to see patterns—like “when I use 500 psi injection pressure, shrinkage is 1.8%; at 550 psi, it’s 1.5%.” That log becomes your cheat sheet, so you don’t have to test every new part from scratch.

Now, I know some of you are thinking, “This sounds like a lot of work—can’t I just guess and adjust?” But let’s be real: LSR molding is already competitive, and tight tolerances are non-negotiable for so many industries (medical, automotive, aerospace, consumer tech). If your shrinkage is off, you’re losing money on rework, missed deadlines, and unhappy clients. As an LSR molder supplier, my job isn’t just to sell machines—it’s to help you make parts that work the first time.

If you’re struggling with shrinkage rates right now, or you’re upgrading your LSR line and want a machine that keeps pressure and temp consistent (no surprises mid-cycle), I’m here to help. Whether you need a toggle machine for high-volume parts, a dual-color machine for multi-material jobs, or a horizontal press for small, precise components, we’ve got the gear, and our team can walk you through setup tweaks specific to your parts. No sales pitches, no jargon—just straight talk to get your shrinkage rates locked in. Reach out, and let’s troubleshoot your process together.

References

  1. International Organization for Standardization. (2018). ISO 10993-5: Biological evaluation of medical devices - Part 5: Tests for in vitro cytotoxicity.
  2. Davidson, R. (2021). Liquid Silicone Rubber Molding: Process Optimization for Low Shrinkage. Journal of Polymer Processing, 36(2), 45-52.
  3. Smith, L. et al. (2022). Mold Design and Temperature Control for Precision LSR Parts. Journal of Manufacturing Processes, 48, 112-119.
  4. Silicone Technology Association. (2023). LSR Material Selection Guide for High-Tolerance Molding.
  5. Thompson, K. (2020). Cycle Time Tuning in LSR Injection Molding: Balancing Speed and Shrinkage. Plastics Engineering, 76(8), 22-27.